go on to boost, to be certain item quality in line with market and buyer standard demands. Our firm has a excellent assurance procedure happen to be established for Fkm Rubber Material, Fpm Viton, Joint Fkm, We sincerely welcome overseas buyers to consult for that long-term cooperation as well as the mutual progress.
factory Outlets for Fkm Gum - FKM High Fluorine content (70%) – Huaxia Shenzhou Detail:

Fluoroelastomer FKM Terpolymer Gum-246 series are the terpolymer of vinylidenefluoride,tetrafluoroethylene and hexafluoropropylene.Because of its high fluorine content,its vulcanized rubber has excellent anti oil property and high thermal stability.It also has good mechanical property and can be used in 275℃ for a long time,in 320℃ for a short time.The property of antil oil and anti acid is better than FKM-26,resistance of FKM246 to oil,ozone,radiation,electricity and flamer is similar with FKM26.

Execution standard:Q/0321DYS 005

FKM246-(3)

Quality Specification

Item 246G Test Method/Standards
Density,g/cm³ 1.89±0.02 GB/T533
Mooney Viscosity,ML(1+10)121℃ 50-60 GB/T1232-1
Tensile Strength,MPa≥ 12 GB/T528
Elongation at break,%≥ 180 GB/T528
Compression Set(200℃,70h),%≤ 30 GB/T7759
Fluorine Content,% 70 /
Characteritics and Application Good chemical resistance and liquid resistance /

Note:The above vulcanization systems are bisphenol AF 

Product Use

FKM246 is widely used in aerospace,automotive,machinery,petrochemical,and other fields.For example,the aircraft static/ dynamic seals materials of hydraulic system and lubrication system;used in drilling equipment and oil pipelines;the chemical industry for equipment,flexible pipe connections,liner of pump or corrosion-resistant sealing material,made of pipes to carry solvents or other media,such as corrosion.

Attention

1.Fluoroelastomer terpolymer rubber has good heat stability under 200℃.It will generate trace decomposition if being put at 200-300′C for a long time,and its decomposing speed accelerates at above 320℃,the decomposition products are mainly toxic hydrogen fluoride and fluorocarbon organic compound.When raw fluorous rubber encounters fire,it will release toxic hydrogen fluoride and fluorocarbon organic compound.

2.FKM cannot be mixed with metal powder such as aluminum powder and magnesium powder,or over10% amine compound,if that happens, temperature will arise and several element will react with FKM,which will damage the equipment and operators.

Package, Transportation and Storage

1.FKM is packed in PE plastic bags,and then loaded into cartons,the net weight of each carton is 20kg.

2.FKM is stored in clean,dry and cool warehouse.It is transported according to non-hazardous chemicals,and should keep away from pollution source,sunshine and water during transportation.

FKM246-(3)
FKM26-(4)


Product detail pictures:

factory Outlets for Fkm Gum - FKM High Fluorine content (70%) – Huaxia Shenzhou detail pictures

factory Outlets for Fkm Gum - FKM High Fluorine content (70%) – Huaxia Shenzhou detail pictures


Related Product Guide:

We are going to dedicate ourselves to providing our esteemed buyers together with the most enthusiastically thoughtful products and services for factory Outlets for Fkm Gum - FKM High Fluorine content (70%) – Huaxia Shenzhou , The product will supply to all over the world, such as: El Salvador, Manila, Argentina, Our products and solutions are sold to the Middle East, Southeast Asia, Africa, Europe, America and other regions, and are favorably appraised by clients. To benefit from our strong OEM/ODM capabilities and considerate services, be sure to contact us today. We will sincerely create and share success with all clients.
  • The factory can meet continuously developing economic and market needs, so that their products are widely recognized and trusted, and that's why we chose this company.
    5 Stars By Agustin from Turkey - 2017.09.26 12:12
    This supplier stick to the principle of "Quality first, Honesty as base", it is absolutely to be trust.
    5 Stars By Sarah from UAE - 2018.12.05 13:53
    Leave Your Message